Press Plates

  • Too smooth sheets have the disadvantage that the laminate between the sheets may flow.
  • Using too smooth sheets also the effect of “bonding” of the pressed laminates appears after lamination and punching.
  • The thickness of 0,8 up to 1 mm is recommended for the press plates. For the pre-lamination of contactless inlays 1,5 mm is widely used